MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Viper-Skin™ Carbon Fiber Composite
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Polyurethane, TS

Material Notes: Viper-Skin™ is the first bi-axial, hybrid carbon and glass fiber polyurethane pre-impregnated system that blends the unsurpassed strength and stiffness of carbon with the ease and use of a moisture-cured, factory-saturated fiber.

Typical Applications:

  • Transmission and distribution pipelines
  • Oil and gas risers
  • Mechanical dents and defects
  • Girth welds on vessels and pipelines
  • Process piping: chemicals, oil, gases, water and steam
Benefits:
  • Moisture-cured polyurethane resin reduces composite preparation time by over 50%
  • Factory-saturation optimizes fiber to resin ration and provides a material with a constant strength property
  • Non-shielding
  • Can be applied to damp, sweating, or immersed surfaces
  • No heating or post-curing required
  • Can be applied to any geometry including, but not limited to elbows, Tees, and flanges
  • Design conforms to ASME PCC-2, ASME B31, ISO TS24817, DOT, API, and CSA Z662 standards for nonmetallic reinforcing solutions

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 18.0 milLaminate
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 83
Flexural Strength 61600 psi
Poissons Ratio 0.218
Shear Strength 6145 psiIn-plane
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 90.0 °C
Minimum Service Temperature, Air -18.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 138 °C
Set time
 20.0 min
@Temperature 32.0 °C
Set time
 40.0 min
@Temperature 24.0 °C
Set time
 75.0 min
@Temperature 16.0 °C
Set time
 120 min
@Temperature 10.0 °C
Set time
Pot Life 30.0 min
Working Life 2.00 min
@Temperature 138 °C
 12.0 min
@Temperature 32.0 °C
 20.0 min
@Temperature 24.0 °C
 40.0 min
@Temperature 16.0 °C
 60.0 min
@Temperature 10.0 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
NRI Syntho-Subsea™ LV Epoxy Primer System
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
E-Glass Fiber, Generic

PNRI033 / 192049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.