MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NRI Syntho-Subsea™ LV Epoxy Primer System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Syntho-Subsea™LV Epoxy, a Kevlar-reinforced tri-polymer, utilizes liquid epoxy, polymer, and aliphatic polyamine curing agents, in order to displace water from wet surfaces.

Typical Applications:

  • Anticorrosive coating, including splash zone and subsea applications
  • Encapsulating coating
  • Pipeline repair
  • Concrete repairs
  • Pipeline anomaly reinforcement and remediation
  • Brush or roller applied
  • All ISO 12944 environments (C1-C5M)
Benefits:
  • Use above- or below-grade, as well as immersion
  • Zero VOC system
  • Chemical resistant coating
  • Excellent abrasive resistance
  • Ships as non-hazardous by USDOT, IATA, and IMO
  • Fully cured in 24 hours

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 41.4 MPa6000 psiASTM D3039
Flexural Strength 31.4 MPa4550 psiASTM D790
Flexural Modulus 0.980352 GPa142.188 ksiASTM D790
Compressive Strength 50.9 MPa7380 psiASTM D695
Shear Strength 12.29 MPa1782 psiLap; ASTM D3163
Abrasion 3434[mg]/1000 cycles, with 1000 gram weights; CS17
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 32.0 °C
2.00 hour
@Temperature 89.6 °F
 240 min
@Temperature 24.0 °C
4.00 hour
@Temperature 75.2 °F
 720 min
@Temperature 16.0 °C
12.0 hour
@Temperature 60.8 °F
 1440 min
@Temperature 10.0 °C
24.0 hour
@Temperature 50.0 °F
Pot Life 20.0 min20.0 min
Working Life  35.0 min
@Temperature 32.0 °C
35.0 min
@Temperature 89.6 °F
 75.0 min
@Temperature 24.0 °C
75.0 min
@Temperature 75.2 °F
 150 min
@Temperature 16.0 °C
150 min
@Temperature 60.8 °F
 225 min
@Temperature 10.0 °C
225 min
@Temperature 50.0 °F
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NRI Syntho-Glass® XT Fiberglass
NRI Viper-Skin™ Carbon Fiber Composite
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber

PNRI013 / 192029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.