MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Syntho-Subsea™ LV Epoxy Primer System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Syntho-Subsea™LV Epoxy, a Kevlar-reinforced tri-polymer, utilizes liquid epoxy, polymer, and aliphatic polyamine curing agents, in order to displace water from wet surfaces.

Typical Applications:

  • Anticorrosive coating, including splash zone and subsea applications
  • Encapsulating coating
  • Pipeline repair
  • Concrete repairs
  • Pipeline anomaly reinforcement and remediation
  • Brush or roller applied
  • All ISO 12944 environments (C1-C5M)
Benefits:
  • Use above- or below-grade, as well as immersion
  • Zero VOC system
  • Chemical resistant coating
  • Excellent abrasive resistance
  • Ships as non-hazardous by USDOT, IATA, and IMO
  • Fully cured in 24 hours

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 41.4 MPaASTM D3039
Flexural Strength 4550 psiASTM D790
Flexural Modulus 142188 psiASTM D790
Compressive Strength 7380 psiASTM D695
Shear Strength 1782 psiLap; ASTM D3163
Abrasion 34[mg]/1000 cycles, with 1000 gram weights; CS17
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 32.0 °C
 4.00 hour
@Temperature 24.0 °C
 12.0 hour
@Temperature 16.0 °C
 24.0 hour
@Temperature 10.0 °C
Pot Life 20.0 min
Working Life 35.0 min
@Temperature 32.0 °C
 75.0 min
@Temperature 24.0 °C
 150 min
@Temperature 16.0 °C
 225 min
@Temperature 10.0 °C
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NRI Syntho-Glass® XT Fiberglass
NRI Viper-Skin™ Carbon Fiber Composite
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
DuPont™ Kevlar® 49 Aramid Fiber
DuPont™ Kevlar® 29 Aramid Fiber

PNRI013 / 192029

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.