MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Pluracol® 2097 Molded Foam Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 2097 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams, one-shot semi-flexible and microcellular foams. HR foams made with Pluracol 2097 in combination with graft polyols, such as Pluracol 4830, process well and are easily crushed. Pluracol 2097 is less reactive than either Pluracol 816 or Pluracol 945.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cc
@Temperature 55.0 °C
 0.999 g/cc
@Temperature 40.0 °C
 1.01 g/cc
@Temperature 25.0 °C
Viscosity 210 cP
@Temperature 55.0 °C
 400 cP
@Temperature 40.0 °C
 840 cP
@Temperature 25.0 °C
Molecular Weight 4800 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.010STI 3063/3161
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.16 J/g-°C
Thermal Conductivity 0.125 W/m-K
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %STI 3062
 
Descriptive Properties
Color<50APHA, STI 3057
 Clear Liquid
CompositionNa & K<5 ppm, STI 3038
Hydroxyl Number34 - 36 mg KOH/gSTI 3007/3162
Unsaturation<0.06 meq/gSTI 3056

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Pluracol® 2100 Slabstock HR Foam Polyol
BASF Pluracol® 2090 Specialty Polyol
BASF Pluracol® 1603 Molded Foam Polyol
Covestro Acclaim® 2200 Polyol
BASF Pluracol® 2086 Slabstock Foam Polyol

PBASG0782 / 132415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.