MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Pluracol® 1603 Molded Foam Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 1603 polyol is a primary hydroxyl terminated polyether polyol containing an LVI inhibitor package making it ideal for molded seating foam applications. It has an actual functionality of 3.0. The high functionality and high primary content provide fast demold times and excellent stability in high water formulations. It can be used with Pluracol 1528FF graft poyol to formulate flexible foams with a wide range of hardnesses and densities.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.00 g/cc
@Temperature 55.0 °C
0.0361 lb/in³
@Temperature 131 °F
 1.01 g/cc
@Temperature 40.0 °C
0.0365 lb/in³
@Temperature 104 °F
 1.02 g/cc
@Temperature 25.0 °C
0.0368 lb/in³
@Temperature 77.0 °F
Viscosity  285 cP
@Temperature 55.0 °C
285 cP
@Temperature 131 °F
 550 cP
@Temperature 40.0 °C
550 cP
@Temperature 104 °F
 1202 cP
@Temperature 25.0 °C
1202 cP
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.060<= 0.060STI 3063/3161
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.070 %<= 0.070 %STI 3062
 
Descriptive Properties
Color<30APHA, STI 3057
 Clear Liquid
CompositionNa & K<11 ppm, STI 3038
Hydroxyl Number29 - 33 mg KOH/gSTI 3007/3162
Unsaturation<0.07 meq/gSTI 3056

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Pluracol® 2097 Molded Foam Polyol
BASF Pluracol® 2090 Specialty Polyol
BASF Pluracol® 1578 Rigid Polyol
BASF Pluracol® 1538 Slabstock Foam Polyol

PBASG0779 / 132412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.