MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Colacryl® TS1414/4 Acrylic Solution Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Flexible resin produced in a slow drying petroleum fraction and designed for printing inks and covercoats on ceramic and glass transfers. Colacryl® TS1414/4 is a butyl methacrylate copolymer system and has reasonable compatibility with medium and long oil alkyds and vinyl resins. The product is compatible with phthalate, sebacate, and maleate plasticisers.

Suggested Uses:
Recommended for use in silk screen printing inks and media for the ceramic industry.

Information provided by Lucite International

Key Words: Butyl Methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Viscosity 20000 - 27500 cP20000 - 27500 cP
 
Descriptive Properties
SolventSolvesso 1000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Colacryl® TS1326 Acrylic Dental Resin
Lucite International Colacryl® PD11SG Acrylic Dental Resin
Lucite International Colacryl® TS1742 Acrylic Dental Resin
Lucite International Colacryl® TS1171 Acrylic Solution Resin
Lucite International Colacryl® D80FC Acrylic Dental Resin

PLUCIT9433 / 150147

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.