MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Colacryl® TS1326 Acrylic Dental Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Colacryl® TS1326 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of temporary crown and bridge materials. It may be used in conjunction with most traditional cold curing dental liquids and is especially suited for use with Colacryl® TS1285 Dental Liquid.

Information provided by Lucite International

Key Words: ethyl methacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 30 - 45 µm30 - 45 µm
Molecular Weight 300000 - 500000 g/mol300000 - 500000 g/mol
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.50 %0.50 %
 
Descriptive Properties
BPO Content (%)0.6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Colacryl® PD11SG Acrylic Dental Resin
Lucite International Colacryl® D60 Acrylic Dental Resin
Lucite International Colacryl® TS1742 Acrylic Dental Resin
Lucite International Colacryl® D80FC Acrylic Dental Resin
Lucite International Colacryl® 1204 Acrylic Solution Resin

PLUCIT9438 / 150152

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.