MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arsenical Admiralty Copper, UNS C44300
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability for forming and bending.

Applications: condenser, evaporator and heat exchanger tubing, condenser tubing plates, distiller tubing, ferrules.

Available as flat products, wire, and tube.

Key Words: Inhibited Admiralty Metal, Admiralty Brass, CDA 443, CZ111, ISO CuZn28Sn1As
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 331 - 379 MPa
Tensile Strength, Yield 124 - 152 MPaDepending on temper
Elongation at Break 65 %in 0 mm.
Creep Strength 0.370 MPa
@Temperature 425 °C,
Time 3.60e+6 sec
0.01%
 1.10 MPa
@Temperature 425 °C,
Time 3.60e+6 sec
0.1%
 3.40 MPa
@Temperature 425 °C,
Time 3.60e+6 sec
1%
 6.90 MPa
@Temperature 315 °C,
Time 3.60e+6 sec
0.01%
 13.4 MPa
@Temperature 315 °C,
Time 3.60e+6 sec
0.1%
 26.0 MPa
@Temperature 315 °C,
Time 3.60e+6 sec
1%
 90.0 MPa
@Temperature 205 °C,
Time 3.60e+6 sec
0.01%
 117 MPa
@Temperature 205 °C,
Time 3.60e+6 sec
0.1%
 130 MPa
@Temperature 205 °C,
Time 3.60e+6 sec
1%
Modulus of Elasticity 110 GPa
 110 GPa
Poissons Ratio 0.38calculated
Fatigue Strength 115 - 125 MPa
@# of Cycles 1.00e+7
source does not state temper
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
 30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa
 40.0 GPa
Charpy Impact 82.4 JCold Drawn and Annealed
 79.7 J
@Temperature -18.0 °C
Cold Drawn and Annealed
 79.9 J
@Temperature -50.0 °C
Cold Drawn and Annealed
 80.3 J
@Temperature -115 °C
Cold Drawn and Annealed
 82.2 J
@Temperature 3.00 °C
Cold Drawn and Annealed
 82.4 J
@Temperature -30.0 °C
Cold Drawn and Annealed
 82.4 J
@Temperature 20.0 °C
Cold Drawn and Annealed
 83.4 J
@Temperature -80.0 °C
Cold Drawn and Annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000690 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 110 W/m-K
@Temperature 20.0 °C
Melting Point 900 - 935 °C
Solidus 900 °C
Liquidus 935 °C
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 600 °C
Hot-Working Temperature 650 - 800 °C
Recrystallization Temperature 300 °CFor 1 mm strip cold rolled hard(50% reduction), from 0.015 mm grain size
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As 0.020 - 0.10 %
Copper, Cu 70 - 73 %
Iron, Fe <= 0.060 %
Lead, Pb <= 0.070 %
Tin, Sn 0.90 - 1.2 %
Zinc, Zn 28 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phosphorized Admiralty Copper, UNS C44400, Cold Drawn and Annealed
Architectural Bronze, UNS C38000
Aluminum Brass Arsenical, UNS C68700
Arsenical Admiralty Copper, UNS C44300, H04 Temper strip
Arsenical Naval brass, UNS C46500

MC44300c1 / 11388

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.