MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Abatron AboCoat 8709-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: AboCoat 8709-2 A/B is a high-solid carbon-epoxy coating with various conductivity ranges widely used in silk-screening.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 79 %
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 200000 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 - 180 min
@Temperature 50.0 - 100 °C
Optional
 >= 1440 min
@Temperature 22.0 - 30.0 °C
Pot Life 800 min
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 15 %of vehicle
 
Descriptive Properties
ColorBlack
Parts by Weight (pbw)100Part A Resin
 40Part B Hardener
ViscosityHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron 8509-1 A/B Carbon-Filled Electrically Conductive Epoxy Compound
Abatron AboWeld 8201-14/AboCure 50-12 Carbon-Filled Electrically Conductive Epoxy Compound
Master Bond EP75-1 Graphite Filled Electrically Conductive Epoxy System
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive
Epoxy Technology EPO-TEK® H44 Gold-Filled, Electrically Conductive Epoxy

PABC859 / 107843

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.