MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics CHO-SEAL V6433 Conductive Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material of choice for extensive fluid resistance; no corrosion resistance.

Molded only

RoHS Compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 4.55 - 5.05 g/cc4.55 - 5.05 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 78 - 9278 - 92ASTM D2240
Tensile Strength at Break >= 2.76 MPa>= 400 psiASTM D412
Elongation at Break >= 50 %>= 50 %ASTM D412
Tear Strength 12.25 kN/m69.90 pliASTM D624
Compression Set <= 45 %
@Temperature 100 °C,
Time 252000 sec
<= 45 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0060 ohm-cm0.0060 ohm-cmas supplied without pressure sensitive adhesive; MIL-DTL-83528
Shielding Effectiveness  >= 90 dB
@Frequency 2.00e+9 Hz
>= 90 dB
@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 90 dB
@Frequency 1e+10 Hz
>= 90 dB
@Frequency 1e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 100 dB
@Frequency 5.00e+8 Hz
>= 100 dB
@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 >= 105 dB
@Frequency 1e+8 Hz
>= 105 dB
@Frequency 1e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.10 W/m-K
@Pressure 2.07 MPa
14.6 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °FFlex TR10; ASTM D1329
 
Descriptive Properties
BinderFluorocarbon/Fluorosilicone
FillerAg/Ni
Heat Aging <0.008 ohm-cm 200°C fir 48 hrs; CEPS-0002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Fluorocarbon Rubber (FPM), Low Temperature Grade
NuSil CF1-3800 Fluorosilicone
Parker Chomerics CHO-THERM® 1677 Thermally Conductive Insulator
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler

PCHOME116 / 28338

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.