MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

NuSil CF1-3800 Fluorosilicone
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Thermally Conductive

Comments: Fuel Resistant

Cure System: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
Tensile Strength at Break 0.860 MPa125 psi
Elongation at Break 50 %50 %
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.25 W/m-K8.68 BTU-in/hr-ft²-°FASTM E1530
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
Working Life 120 min120 min
 
Descriptive Properties
ColorWhite
Mix Ratio15:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-THERM® 1677 Thermally Conductive Insulator
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber
Parker Chomerics CHO-SEAL 6370 Conductive Elastomer
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material

PNUSIL092 / 141816

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.