MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.37 - 1.69 g/ccAverage value: 1.62 g/cc Grade Count:60
Filler Content 30.0 %Average value: 30.0 % Grade Count:15
Water Absorption 0.0200 - 1.30 %Average value: 0.154 % Grade Count:11
Moisture Absorption at Equilibrium 0.00200 - 0.0600 %Average value: 0.0340 % Grade Count:8
Water Absorption at Saturation 0.0300 - 0.0800 %Average value: 0.0467 % Grade Count:3
Linear Mold Shrinkage -0.00100 - 0.00400 cm/cmAverage value: 0.000804 cm/cm Grade Count:47
 0.00100 - 0.00100 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00100 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00200 - 0.00900 cm/cmAverage value: 0.00551 cm/cm Grade Count:40
 0.00500 - 0.00500 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00500 cm/cm Grade Count:2
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 40.0 - 100Average value: 72.1 Grade Count:21
Hardness, Rockwell R 105 - 118Average value: 109 Grade Count:6
Tensile Strength, Ultimate 92.0 - 210 MPaAverage value: 149 MPa Grade Count:60
 14.0 - 250 MPa
@Temperature -40.0 - 250 °C
Average value: 86.2 MPa Grade Count:3
 14.0 - 250 MPa
@Thickness 0.800 - 3.17 mm
Average value: 86.2 MPa Grade Count:3
Elongation at Break 1.00 - 6.20 %Average value: 2.16 % Grade Count:58
 0.800 - 1.40 %
@Temperature -40.0 - 250 °C
Average value: 1.14 % Grade Count:1
 0.800 - 1.40 %
@Thickness 1.60 - 1.60 mm
Average value: 1.14 % Grade Count:1
Modulus of Elasticity 7.00 - 23.5 GPaAverage value: 14.4 GPa Grade Count:47
 3.40 - 29.0 GPa
@Temperature -40.0 - 250 °C
Average value: 12.3 GPa Grade Count:3
 3.40 - 29.0 GPa
@Thickness 1.60 - 3.17 mm
Average value: 12.3 GPa Grade Count:3
Flexural Yield Strength 124 - 300 MPaAverage value: 199 MPa Grade Count:53
 17.0 - 340 MPa
@Temperature -40.0 - 250 °C
Average value: 105 MPa Grade Count:3
 17.0 - 340 MPa
@Thickness 0.800 - 3.17 mm
Average value: 105 MPa Grade Count:3
Flexural Modulus 6.60 - 26.0 GPaAverage value: 13.6 GPa Grade Count:58
 2.80 - 25.0 GPa
@Temperature -40.0 - 250 °C
Average value: 9.10 GPa Grade Count:3
 2.80 - 25.0 GPa
@Thickness 0.800 - 3.17 mm
Average value: 9.10 GPa Grade Count:3
Flexural Strain at Break 1.80 - 4.20 %Average value: 2.65 % Grade Count:6
Compressive Yield Strength 38.0 - 150 MPaAverage value: 107 MPa Grade Count:20
Compressive Modulus 6.00 - 23.5 GPaAverage value: 16.5 GPa Grade Count:14
Shear Strength 51.0 - 68.0 MPaAverage value: 58.2 MPa Grade Count:3
Izod Impact, Notched 0.167 - 4.00 J/cmAverage value: 1.57 J/cm Grade Count:19
 1.10 - 4.90 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 2.67 J/cm Grade Count:3
 1.10 - 4.90 J/cm
@Thickness 0.800 - 3.17 mm
Average value: 2.67 J/cm Grade Count:3
Izod Impact, Unnotched 3.47 J/cm - NBAverage value: 6.10 J/cm Grade Count:10
 5.55 - 475 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 294 J/cm Grade Count:3
 5.55 - 475 J/cm
@Thickness 0.800 - 3.17 mm
Average value: 294 J/cm Grade Count:3
Izod Impact, Notched (ISO) 4.00 - 67.0 kJ/m²Average value: 22.0 kJ/m² Grade Count:29
 20.0 - 20.0 kJ/m²
@Temperature -40.0 - -40.0 °C
Average value: 20.0 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 15.0 - 56.6 kJ/m²Average value: 32.3 kJ/m² Grade Count:8
 30.0 - 30.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 30.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 0.600 - 8.60 J/cm²Average value: 3.33 J/cm² Grade Count:28
 2.20 - 3.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 2.52 J/cm² Grade Count:6
Charpy Impact, Notched 0.500 - 4.30 J/cm²Average value: 2.17 J/cm² Grade Count:37
 1.50 - 3.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 2.29 J/cm² Grade Count:7
Tensile Creep Modulus, 1 hour 12600 - 19600 MPaAverage value: 15100 MPa Grade Count:6
Tensile Creep Modulus, 1000 hours 10900 - 15800 MPaAverage value: 12900 MPa Grade Count:6
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 100 - 1.00e+17 ohm-cmAverage value: 6.57e+15 ohm-cm Grade Count:39
Surface Resistance 10.0 - 1.00e+17 ohmAverage value: 7.46e+15 ohm Grade Count:34
Dielectric Constant 2.70 - 5.60Average value: 3.99 Grade Count:37
 4.10 - 5.00
@Temperature 100 - 250 °C
Average value: 4.55 Grade Count:5
 4.10 - 5.00
@Frequency 1000 - 1.00e+9 Hz
Average value: 4.55 Grade Count:5
Dielectric Strength 16.1 - 56.0 kV/mmAverage value: 33.8 kV/mm Grade Count:32
 26.0 - 41.0 kV/mm
@Temperature 120 - 200 °C
Average value: 32.1 kV/mm Grade Count:3
 26.0 - 41.0 kV/mm
@Thickness 0.800 - 3.20 mm
Average value: 32.1 kV/mm Grade Count:3
Dissipation Factor 0.00400 - 0.340Average value: 0.0215 Grade Count:36
 0.00500 - 0.0450
@Temperature 100 - 250 °C
Average value: 0.0171 Grade Count:5
 0.00500 - 0.0450
@Frequency 1000 - 1.00e+9 Hz
Average value: 0.0171 Grade Count:5
Arc Resistance 124 - 300 secAverage value: 151 sec Grade Count:15
Comparative Tracking Index 100 - 250 VAverage value: 175 V Grade Count:34
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.00 - 24.0 µm/m-°CAverage value: 4.46 µm/m-°C Grade Count:35
 -5.00 - 6.00 µm/m-°C
@Temperature 55.0 - 260 °C
Average value: 1.04 µm/m-°C Grade Count:7
 -5.00 - 6.00 µm/m-°C
@Thickness 2.00 - 4.00 mm
Average value: 1.04 µm/m-°C Grade Count:7
CTE, linear, Transverse to Flow 6.00 - 88.0 µm/m-°CAverage value: 54.4 µm/m-°C Grade Count:34
 71.0 - 110 µm/m-°C
@Temperature 55.0 - 260 °C
Average value: 90.4 µm/m-°C Grade Count:7
 71.0 - 110 µm/m-°C
@Thickness 2.00 - 4.00 mm
Average value: 90.4 µm/m-°C Grade Count:7
Melting Point 280 - 370 °CAverage value: 325 °C Grade Count:44
Deflection Temperature at 0.46 MPa (66 psi) 210 - 305 °CAverage value: 268 °C Grade Count:18
Deflection Temperature at 1.8 MPa (264 psi) 160 - 310 °CAverage value: 262 °C Grade Count:61
Deflection Temperature at 8.0 MPa 89.0 - 244 °CAverage value: 183 °C Grade Count:16
Vicat Softening Point 138 - 252 °CAverage value: 189 °C Grade Count:17
Glass Transition Temp, Tg 120 °CAverage value: 120 °C Grade Count:6
UL RTI, Electrical 130 - 240 °CAverage value: 224 °C Grade Count:11
UL RTI, Mechanical with Impact 130 - 220 °CAverage value: 204 °C Grade Count:11
UL RTI, Mechanical without Impact 130 - 240 °CAverage value: 233 °C Grade Count:8
Flammability, UL94 V-0Grade Count:53
Oxygen Index 38.0 - 51.0 %Average value: 44.8 % Grade Count:19
Glow Wire Test 800 - 960 °CAverage value: 923 °C Grade Count:4
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 375 °CAverage value: 163 °C Grade Count:24
Nozzle Temperature 290 - 365 °CAverage value: 330 °C Grade Count:5
Die Temperature 290 - 375 °CAverage value: 327 °C Grade Count:20
Melt Temperature 270 - 399 °CAverage value: 325 °C Grade Count:49
Mold Temperature 30.0 - 160 °CAverage value: 85.9 °C Grade Count:36
Injection Velocity 150 mm/secAverage value: 150 mm/sec Grade Count:11
Drying Temperature 149 - 170 °CAverage value: 151 °C Grade Count:40
Moisture Content 0.0100 %Average value: 0.0100 % Grade Count:32
Dew Point -28.9 °CAverage value: -28.9 °C Grade Count:4
Injection Pressure 34.5 - 150 MPaAverage value: 96.2 MPa Grade Count:25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled

O2243 / 77946

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.