MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos N01G-02 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: N01G-02 is a low melt flow rate polypropylene impact copolymer designed for blow molding, extrusion, and compounding applications. The grade benefits from a very high impact resistance at room and low temperatures and a general purpose additive package. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

Key Words: Very high impact resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 85ASTM D785
Tensile Strength at Break 2370 psi2 in/min; ASTM D638
Tensile Strength, Yield 3710 psi2 in/min; ASTM D638
Elongation at Break 285 %2 in/min; ASTM D638
Elongation at Yield 8.2 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 174 ksiASTM D790A
Izod Impact, Notched 1.60 ft-lb/in
@Temperature -20.0 °C
ASTM D256
 NB
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 197 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 123 °FASTM D648
Vicat Softening Point 304 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 59 %60° Angle; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Instrumented ImpactDuctile at -20°C
 Ductile at 23°C
processBlow Molding
 Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N01N-00 Polypropylene Impact Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos N05G-00 Polypropylene Impact Copolymer

PINEOS920 / 171735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.