MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mo-Sci Corporation GL 1756 Porous Wall Hollow Glass Microspheres
Categories: Ceramic; Glass

Material Notes: Porous wall hollow microspheres provide a porous shell for introduction or release of liquids. The porous shells have a microstructure similar to Vycor and are composed of open channels from the outer shell to the inner shell. The porous wall hollow microspheres are ~98% porous with pore sizes ranging from 100Å to 3000Å and a shell thickness of ~1µm. Typical applications of GL1756 spheres including: filtration, waste remediation, drug delivery, batteries, a variety of biological diagnostic uses, and bone regeneration to name a few.

Information provided by Mo-Sci Corporation.

Key Words: PWHGM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 g/cc0.0145 lb/in³dry spheres
Porosity >= 90 %>= 90 %
Pore Size 0.0100 - 0.300 microns0.000394 - 0.0118 mil
 
Component Elements PropertiesMetricEnglishComments
B2O3 5.0 - 15 %5.0 - 15 %
Other 1.0 - 10 %1.0 - 10 %
SiO2 75 - 90 %75 - 90 %
 
Descriptive Properties
Shell Thickness (µm)1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMOSCI9022 / 200237

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.