MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema OREVAC® 18722 Maleic Anhydride Modified Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: OREVAC 18722 is a maleïc anhydride modified PP based resin. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins. OREVAC 18722 is an extrusion adhesive to be used in coextrusion technologies. As adhesive, OREVAC 18722 has been designed to develop adhesion in coextrusion between PP and EVOH or PP and PA .

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Index of Compound 7.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 143 °CDSC
Vicat Softening Point 115 °CISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 240 °C
Adapter Temperature 230 °C
Die Temperature 240 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema OREVAC® 18729 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18750 Maleic Anhydride Modified Polypropylene
Arkema OREVAC® 18707 Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18732P Grafted Maleic Anhydride Polypropylene
Arkema OREVAC® 18751 Maleic Anhydride Modified Polypropylene

PARKG136 / 80100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.