MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arkema OREVAC® 18751 Maleic Anhydride Modified Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description

OREVAC 18751 is a coextrusion coating adhesive based on a maleic anhydride modified polypropylene resin. It combines the processability of an extrusion coating resin with the thermal resistance of polypropylene. OREVAC 18751 is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyolefins.

Applications

OREVAC 18751 is a tie resin to be used in extrusion coating and extrusion lamination technologies. It has been designed to develop adhesion in these processes onto substrates like aluminum foil, paper, or PP films and in coextrusion with resins like PP and PA. OREVAC 18751 exhibits excellent processing properties, particularly regarding drawability, neck-in and melt stability. In addition to adhesive properties, the special formulation of OREVAC 18751 allows to design aluminium lids for PP or PP coated cups and containers with controlled opening forces.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Melt Index of Compound 37 g/10 min
@Load 2.16 kg,
Temperature 230 °C
37 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.0 MPa3480 psiISO R 527
Elongation at Break 500 %500 %ISO R 527
Tensile Modulus 0.880 GPa128 ksiISO R 527
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FDSC
Vicat Softening Point 138 °C280 °FISO 306
 
Processing PropertiesMetricEnglishComments
Feed Temperature 275 °C527 °F
Adapter Temperature 275 °C527 °F
Die Temperature 275 °C527 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema OREVAC® 18722 Maleic Anhydride Modified Polypropylene
Arkema OREVAC® 18750 Maleic Anhydride Modified Polypropylene
Arkema OREVAC® 18760 Grafted Maleic Anhydride Polypropylene
LyondellBasell Hostacom DYS 707N T 3130 (BASALT) Polypropylene, Impact Modified; Molded/Extruded
Arkema OREVAC® 18732 Grafted Maleic Anhydride Polypropylene

PARKG145 / 80102

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.