MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom DYS 707N T 3130 (BASALT) Polypropylene, Impact Modified; Molded/Extruded
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Hostacom DYS 707N T 3130 is an unfilled impact modified polypropylene, with good processability and excellent impact/stiffness balance. Product is available as a customized color matched, pellet form. This grade is delivered in 3130 color version. Applications: Interior Trims

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³Method A; ISO 1183-1
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 230 °C
23 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 18.0 MPa2610 psiISO 527-1,-2
Flexural Modulus 1.15 GPa167 ksiISO 178
Charpy Impact, Notched  0.450 J/cm²
@Temperature -40.0 °C
2.14 ft-lb/in²
@Temperature -40.0 °F
ISO 179-1/1eA
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C169 °Funannealed; ISO 75B-1,-2
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Bynel® 50E725 Anhydride Modified Polypropylene
Braskem TR3350MS Polypropylene High Impact Random Copolymer
Arkema OREVAC® 18751 Maleic Anhydride Modified Polypropylene
Arkema OREVAC® 18750 Maleic Anhydride Modified Polypropylene
Arkema OREVAC® 18722 Maleic Anhydride Modified Polypropylene

PEQT7748 / 219386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.