MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro MAKROFOL® LM 905 2-4 160009 Polycarbonate Films
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol LM 905 2-4 160009 is an extruded polycarbonate film.

Properties / Applications: Makrofol LM 905 2-4 160009 is an extruded polycarbonate film filled with light-scattering agent. It displays a smooth homogenous illumination of the front side of a backlight part even if a point source is applied. Typical applications are automotive instrument panels and backlight displays. Makrofol LM 905 2-4 160009 is available in standard thicknesses of 0.012" and 0.020" (300 microns and 500 microns). The surface structure of Makrofol LM 905 2-4 160009 is one side very fine matte and one side fine matte. As with any product, use of Makrofol LM 905 2-4 160009 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 1183, Method C
Water Absorption 0.20 %0.20 %following ISO 62
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 115 %>= 115 %ISO 527-1,-3
Film Elongation at Break, TD >= 115 %>= 115 %ISO 527-1,-3
Tensile Modulus >= 2.30 GPa>= 334 ksiTD; ISO 527-1,-3
 >= 2.40 GPa>= 348 ksiMD; ISO 527-1,-3
Film Tensile Strength at Break, MD >= 70.0 MPa>= 10200 psiISO 527-1,-3
Film Tensile Strength at Break, TD >= 70.0 MPa>= 10200 psiISO 527-1,-3
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+16 ohm1.00e+16 ohmfollowing DIN IEC 60093
 
Optical PropertiesMetricEnglishComments
Haze  100 %
@Wavelength 300 nm
100 %
@Wavelength 300 nm
back surface; ASTM D 1003
 100 %
@Wavelength 300 nm
100 %
@Wavelength 300 nm
top surface; ASTM D 1003
 100 %
@Wavelength 500 nm
100 %
@Wavelength 500 nm
back surface; ASTM D 1003
 100 %
@Wavelength 500 nm
100 %
@Wavelength 500 nm
top surface; ASTM D 1003
Gloss <= 6.0 %<= 6.0 %60°, back surface; ISO 2813
 >= 80 %>= 80 %60°, top surface; ISO 2813
Transmission, Visible  73 %
@Wavelength 500 nm
73 %
@Wavelength 500 nm
back surface; ISO 13467-2
 73 %
@Wavelength 500 nm
73 %
@Wavelength 500 nm
top surface; ISO 13467-2
UV Transmittance  78 %
@Wavelength 300 nm
78 %
@Wavelength 300 nm
top surface; ISO 13467-2
 81 %
@Wavelength 300 nm
81 %
@Wavelength 300 nm
back surface; ISO 13467-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 1-1 000000 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® ID 6-2 laserable Polycarbonate
Covestro Makrofol® ID 4-4 white Polycarbonate

PCOVEST0813 / 202596

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.