MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hytrel® RS 40F5 NC010 TPC-ET
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D, Renewably Sourced, Medium Viscosity Polyester Elastomer

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4, 2577
 0.010 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4, 2577
 0.0080 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 220 °C
cm³/10min Volumetric; ISO 1133
 9.0 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 3315s; ISO 48-4
 <= 37ISO 48-4
Tensile Stress at Strain 2.10 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 3.50 MPa
@Strain 10 %
ISO 527-1/-2
 6.70 MPa
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 50.0 MPaISO 178
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature -40.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature 23.0 °C
ISO 179/1eA
Tear Strength 101 kN/mparallel; ISO 34-1
 103 kN/mnormal; ISO 34-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 210 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 200 µm/m-°CISO 11359-1/-2
Melting Point 190 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -95.0 °CPuncture test - ductile/brittle transition temperature; ISO 6603-2
 -95.0 °CISO 974
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
Oxygen Index 20 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 °COptimum, Extrusion
 210 - 225 °CRange, Extrusion
 225 °COptimum, Injection
 220 - 250 °CRange, Injection
Mold Temperature 30.0 - 40.0 °CInjection
 40.0 °COptimum, Injection
Drying Temperature 100 °CInjection
 90.0 - 110 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
AdditivesBiobased
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
FMVSS ClassSEISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 3078 TPC-ET
Celanese Hytrel® 4068 TPC-ET
Celanese Hytrel® RS 40F3 NC010 TPC-ET
Celanese Hytrel® HTR8163HVBK TPC-ET
Celanese Hytrel® HTR8206 TPC-ET

PDSX5229 / 197869

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.