MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® HTR8163HVBK TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for Extrusion

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Melt Density 1.06 g/cc
@Temperature 240 °C
0.0383 lb/in³
@Temperature 464 °F
Linear Mold Shrinkage, Flow 0.019 cm/cm0.019 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4, 2577
Melt Flow  5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
cm³/10min Volumetric; ISO 1133
 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 606015s; ISO 48-4
 <= 64<= 64ISO 48-4
Tensile Stress at Strain  12.0 MPa
@Strain 5.0 %
1740 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 17.5 MPa
@Strain 10 %
2540 psi
@Strain 10 %
ISO 527-1/-2
 21.0 MPa
@Strain 50 %
3050 psi
@Strain 50 %
ISO 527-1/-2
 23.0 MPa
@Strain 100 %
3340 psi
@Strain 100 %
ISO 527-1/-2
 32.0 MPa
@Strain 300 %
4640 psi
@Strain 300 %
ISO 527-1/-2
Tensile Modulus 0.340 GPa49.3 ksiISO 527-1/-2
Flexural Modulus 0.350 GPa50.8 ksiISO 178
Poissons Ratio 0.480.48
Izod Impact, Notched (ISO)  7.50 kJ/m²
@Temperature -40.0 °C
3.57 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  0.850 J/cm²
@Temperature -40.0 °C
4.04 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 13.0 J/cm²
@Temperature 23.0 °C
61.9 ft-lb/in²
@Temperature 73.4 °F
Partial Break; ISO 179/1eA
Tensile Creep Modulus, 1 hour 310 MPa45000 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 260 MPa37700 psi1000h; ISO 899-1
Tear Strength 185 kN/m1060 plinormal; ISO 34-1
 200 kN/m1140 pliparallel; ISO 34-1
Abrasion 110110mm3; ISO 4649
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 220 µm/m-°C122 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 170 µm/m-°C94.4 µin/in-°FISO 11359-1/-2
Specific Heat Capacity 2.09 J/g-°C
@Temperature 240 °C
0.500 BTU/lb-°F
@Temperature 464 °F
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 240 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 464 °F
Melt
Melting Point 210 °C410 °F10°C/min; ISO 11357-1/-3
Brittleness Temperature -70.0 °C-94.0 °FISO 974
Flame Spread 17.0 mm/min
@Thickness 1.00 mm
0.669 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 °C446 °FOptimum, Extrusion
 225 - 240 °C437 - 464 °FRange, Extrusion
 240 °C464 °FOptimum, Injection
 230 - 260 °C446 - 500 °FRange, Injection
Mold Temperature 45.0 °C113 °FOptimum, Injection
 45.0 - 55.0 °C113 - 131 °FInjection
Drying Temperature 110 °C230 °FInjection
 100 - 120 °C212 - 248 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 3.00 - 4.00 hour3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassSE/BISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET
DuPont Mobility and Materials Hytrel® HTR8139BK TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET

PDSX5209 / 197849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.