MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Hytrel® HTR8163HVBK TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for Extrusion

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccISO 1183
Melt Density 1.06 g/cc
@Temperature 240 °C
Linear Mold Shrinkage, Flow 0.019 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4, 2577
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
cm³/10min Volumetric; ISO 1133
 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6015s; ISO 48-4
 <= 64ISO 48-4
Tensile Stress at Strain 12.0 MPa
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 17.5 MPa
@Strain 10 %
ISO 527-1/-2
 21.0 MPa
@Strain 50 %
ISO 527-1/-2
 23.0 MPa
@Strain 100 %
ISO 527-1/-2
 32.0 MPa
@Strain 300 %
ISO 527-1/-2
Tensile Modulus 340 MPaISO 527-1/-2
Flexural Modulus 350 MPaISO 178
Poissons Ratio 0.48
Izod Impact, Notched (ISO) 7.50 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 NB
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact, Notched 8.50 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 130 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
Tensile Creep Modulus, 1 hour 310 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 260 MPa1000h; ISO 899-1
Tear Strength 185 kN/mnormal; ISO 34-1
 200 kN/mparallel; ISO 34-1
Abrasion 110mm3; ISO 4649
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 220 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 170 µm/m-°CISO 11359-1/-2
Specific Heat Capacity 2.09 J/g-°C
@Temperature 240 °C
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature 240 °C
Melt
Melting Point 210 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -70.0 °CISO 974
Flame Spread 17.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °COptimum, Extrusion
 225 - 240 °CRange, Extrusion
 240 °COptimum, Injection
 230 - 260 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 110 °CInjection
 100 - 120 °CExtrusion
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
 3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassSE/BISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Hytrel® HTR8136BK TPC-ET
DuPont Mobility and Materials Hytrel® HTR8139BK TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET

PDSX5209 / 197849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.