MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit® 72-00015/72-00016 Conductive Silver-Filled Grease
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: TECKNIT CONDUCTIVE GREASE is a highly conductive silver-filled silicone grease which contains no carbon or graphite. The material will maintain its electrical and lubricating properties over a broad environmental range. These conditions and properties include high and low temperatures, excellent resistance to moisture and humidity, inertness to many chemicals, ozone and radiation. TECKNIT CONDUCTIVE GREASE is a viscous paste which can be applied to vertical or overhead surfaces without dripping or running at elevated operating temperatures.

Application Information: TECKNIT CONDUCTIVE GREASE is used on power substation switches and in suspension insulators to reduce EMI noise. It also reduces make-break arcing and pitting of the sliding metal contact surfaces of switches and fills in existing pitted areas with silver/ silicone. In addition, normally closed switches are prevented from sticking due to corrosion or icing. The grease is effective in maintaining a continuous electrical path between contact surfaces which connections of power insulators, which if allowed to arc, can give rise to EMI noise. TECKNIT CONDUCTIVE GREASE is designed to maintain low resistance electrical contact and thereby maintain equipment operation over extended harsh environmental conditions, helping to deliver continuous electrical service.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.20 ohm-cm<= 0.20 ohm-cmQAP-1017
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Descriptive Properties
ColorSilver Gray
ConsistencyLight Paste
FillerAg/Glass
Final ConditionNon-Setting
Number of ComponentsOne
Pot LifeIndefiniteat 25°C
ResinSilicone
Shelf LifeUnopened Container

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay GEROPON® SDS Surfactant
DuPont MOLYKOTE® PG-75 GREASE
DuPont MOLYKOTE® 822M GREASE
DuPont MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM
Dow MOLYKOTE® 1292 LONG LIFE BEARING GREASE

PCHOME410 / 131120

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.