MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont MOLYKOTE® 822M GREASE
Categories: Fluid; Lubricant; Lithium Gellant; Silicone Base

Material Notes: Former Dow Corning product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc
@Temperature 25.0 °C
1.03 g/cc
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Dropping Point 210 °C410 °F
 
Descriptive Properties
Appearancetranslucent
Colorwhite
NLGI Number1-2
Thickening Systemlithium soap

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil G-9000 Silicone Grease
NuSil CV-9052 Dampening Fluid/Lubricant/Grease
Lord Adhesives Thermoset™ TC-228 Thermally Conductive Grease
DuPont MOLYKOTE® PG-75 GREASE
DuPont MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM

PDOWCO261 / 105962

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.