MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Polykemi AB SCANMID 6 B12^ NH11L Nylon 6, Flame Retardant, Halogen Free
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes:

Information provided by Polykemi AB

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm0.011 - 0.013 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.011 - 0.013 cm/cm0.011 - 0.013 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Time 15.0 sec
80
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break <= 78.0 MPa<= 11300 psiISO/R527
Elongation at Break 10 %10 %ISO/R527
Flexural Strength <= 114 MPa<= 16500 psiISO 178
Flexural Modulus 3.40 GPa
@Temperature 23.0 °C
493 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C374 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °F120°C/h; ISO 75/1
Vicat Softening Point  197 °C
@Load 5.001 kg
387 °F
@Load 11.03 lb
50°C/h; ISO 306
 213 °C
@Load 1.00 kg
415 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Glow Wire Test 850 °C
@Thickness 0.800 mm
1560 °F
@Thickness 0.0315 in
IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Epsan Eplamid 6 GX0 20 NC Q1C0B601 Polyamide 6, Halogen Free
Epsan Eplamid 6 GV0 20 NC Q1C0C001 Polyamide 6, Halogenated
Envalior Durethan® DP 2851/30 H3.0 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Flame Retardant, Dry

PPOLYK103 / 122828

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.