MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description

Superlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used in watercraft, large containers, and refuse cart applications.

NOTE: Physical properties are based on rotationally molded samples from unpigmented resins. Density and ESCR tests were performed on compression molded samples.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.952 g/ccASTM D792
Melt Flow 4.0 g/10 min2.16/190; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3600 psi2 in/min; ASTM D638
Elongation at Break >= 195 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 160000 psiASTM D790
Impact Test 65.0 ft-lb
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM impact
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CASTM D648
 
Descriptive Properties
UV StabilizationUV-8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
ICO Polymers ICOTEX™ 520-5005 1000 Micron EVA Powder
ICO Polymers ICOTEX™ 520-5004 1000 Micron EVA Powder
ICO Polymers ICORENE™ 195-1326 LMDPE Rotational Molding Resin
ICO Polymers ICORENE™ 195-1325 LMDPE Rotational Molding Resin

PASHU349 / 25313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.