MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ICO Polymers ICORENE™ 195-1325 LMDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Description: ICORENE 195-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness.
Key Characteristics: good physical properties, easy molding, controlled release.
Applications: This ICORENE® grade is particularly sutiable for use in general purpose applications.

Information provided by ICO Polymers.

A Schulman acquired ICO, Inc. in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ASTM D1505
ESCR 10% Igepal® 10 hour10 hourF50; ASTM D1693
Melt Index of Compound 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 19.0 MPa2760 psi50 mm/min; ASTM D638
Elongation at Break 900 %900 %50 mm/min; ASTM D638
Flexural Modulus 0.690 GPa100 ksi1.3 mm/min; ASTM D790
Impact 19
@Temperature -20.0 °C
19
@Temperature -4.00 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14
 
Descriptive Properties
UV Light Weatherometer Test8000 hoursASTM G26

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
ICO Polymers ICOTEX™ 520-5005 1000 Micron EVA Powder
ICO Polymers ICOTEX™ 520-5004 1000 Micron EVA Powder

PICO090 / 48063

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.