MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate
Categories: Ceramic; Machinable Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Machined easily to close tolerances and can be used as-is or fired to increase temperature resistance and improve mechanical strength. Used for prototyping and small production runs of electrical and thermal insulators and brazing and heat-treating fixtures. Standard plates from ¼” to 1” thick × 12” × 12”; rods from ¼” to 4” diameter × 12”; bars from 1” × 1” to 4” × 4” × 12”.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Water Absorption 2.5 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 39
Flexural Strength 4000 psi
Compressive Strength 12000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 5.8
@Frequency 1e+6 Hz
Dielectric Strength 80.0 V/mil
Dissipation Factor 0.060
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.50 µin/in-°F
@Temperature 20.0 °C
Thermal Conductivity 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1000 °FOxidizing
Maximum Service Temperature, Inert 537 °C
 537 °CVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alclad Aluminum 3003-H12
Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Aremco AREMCOLOX™ 502-1550 (Low Density) Machinable Zirconium Phosphate
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic
Aremco AREMCOLOX™ 502-1550 (Med. Density) Machinable Zirconium Phosphate

CAREM03 / 544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.