MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Offers higher temperature resistance and improved mechanical strength over 502-1100-UF. Used for prototyping and small production runs of electrical and thermal insulators, such as sleeves and washers, and brazing and heat-treating fixtures. Recommended for producing insulators, standoffs, feed-thrus, furnace carriers, and brazing fixtures.

Vendors: Aremco offers a range of machinable ceramics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/cc
Water Absorption 2.3 %2.3 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 4545
Flexural Strength 68.9 MPa10000 psi
Compressive Strength 172 MPa25000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Constant 5.3
@Frequency 1e+6 Hz
5.3
@Frequency 1e+6 Hz
Dielectric Strength 3.94 kV/mm100 kV/in
Dissipation Factor 0.053
@Frequency 1e+6 Hz
0.053
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.22 µm/m-°C
@Temperature 20.0 °C
2.90 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.30 W/m-K9.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1150 °C2100 °FOxidizing
Maximum Service Temperature, Inert 1150 °C2100 °F
 1150 °C2100 °FVacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Thorium, Th
MarkeTech Magnesium Oxide (MgO) Single Crystal Substrate
MarkeTech Zirconium Oxide Ceramic, Zirconia MgO Stabilized

CAREM04 / 545

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.