MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos R01C-01 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Blow Molding Grade; Polypropylene, Impact Modified; Molded/Extruded; Polypropylene, Sheet/Thermoforming Grade

Material Notes: This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance and refrigerator temperature impact properties can benefit from its use. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Thermoformed packaging (cups, containers, lidding)
  • Extrusion blow molded containers and bottles
  • Extruded sheet and profiles

    Benefits
  • Excellent clarity
  • Excellent processability
  • Good impact resistance at room and refrigerator temperatures

Information provided by Ineos Olefins & Polymers USA

Key Words: Good see-through clarity combined with good heat resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 81Injection Molded; ASTM D785
Tensile Strength at Break 2740 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 4270 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 170 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 13 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 159000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.500 ft-lb/in
@Temperature 3.89 °C
Injection Molded; ASTM D256
 6.40 ft-lb/in
@Temperature 22.8 °C
Injection Molded; ASTM D256
Izod Impact, Notched (ISO) 1.24 ft-lb/in²
@Temperature 3.89 °C
Area, Injection Molded; ASTM D256
 15.9 ft-lb/in²
@Temperature 22.8 °C
Area, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 190 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 271 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 16 %
@Thickness 1.27 mm
ASTM D1003
Gloss 97 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessBlow Molding
 Extrusion
 Thermoforming

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos R01C-00 Polypropylene Random Copolymer
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N20G-00 Polypropylene Impact Copolymer
Ineos R01A-00 Polypropylene Random Copolymer
Ineos N05U-00 Polypropylene Impact Copolymer

PINEOS064 / 99385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.