MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unifrax Foamfrax® Grade III Fiber Insulation
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic binder, and an organic foaming binder. Foamfrax Insulation is easily installed at the job site by trained contractors using the special Foamfrax installation machinery. The interlocking network of fibers provides a strong, uniform monolithic structure having excellent thermal insulating properties, very low heat storage, and excellent resistance to thermal shock. Foamfrax Insulation is unaffected by most chemicals except hydrofluoric acid, phosphoric acid, and concentrated alkalies.

    Characteristics
  • Speed and ease of installation
  • Low rebound during installation
  • Low thermal conductivity
  • Low thermal shrinkage
  • Low heat storage
  • Excellent thermal shock resistance
  • Good chemical resistance
  • Good sound absorption

    Principal Applications
  • Furnace linings (reformers, boilers, kilns, heat treating furnaces, etc.)
  • Vessel linings (incinerators, flues, ducts and stacks)
  • Furnace refractory upgrades (Lining over Refractory (LOR), Fiber over Fiber (FOF))
  • Low mass kiln car decks
  • Ladle preheat stands
  • Backup for high-density gunned refractories
  • Boiler tube wall insulation
  • Furnace lining maintenance (gunning gaps, cracks and voids)
  • Fire protection

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/ft³Installed Fired
 16.0 lb/ft³Installed Wet
Loss On Ignition 0.75 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1538 °CRecommended Operating Temperature
Shrinkage <= 3.0 %
@Time 86400 sec
at operating temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 59 - 63 %
H2O, Water 50 %At Installation
SiO2 36 - 40 %
 
Descriptive Properties
ColorWhite (Fired)
Fiber Diameter (microns)1-3.5
Temperature Grade (°C)1649
Trace Elements (%)<2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool HP Veneering Module Thermal Ceramic
Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
Morgan Advanced Ceramics Kaowool C Veneering Module Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

CUNIF101 / 97873

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.