MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Kaowool C Veneering Module Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Kaowool® Veneering modules, HP, ZR, C and polycrystalline Denka® Veneering Modules are made from high temperature grade ceramic fibers or high alumina fibers. The modules are fabricated into 12" x 12" (305 mm x 305 mm) blocks using fiber strips turned edge-grain and slightly compressed with a gauze-type wrap.

Applications:

  • Forge furnace
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 g/cc0.00462 lb/in³
 0.160 g/cc0.00578 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0800 W/m-K
@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 128kg/m3; ASTM C201
 0.0800 W/m-K
@Temperature 260 °C
0.555 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 160kg/m3; ASTM C201
 0.140 W/m-K
@Temperature 538 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 160kg/m3; ASTM C201
 0.160 W/m-K
@Temperature 538 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 128kg/m3; ASTM C201
 0.240 W/m-K
@Temperature 816 °C
1.67 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 160kg/m3; ASTM C201
 0.280 W/m-K
@Temperature 816 °C
1.94 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 128kg/m3; ASTM C201
 0.350 W/m-K
@Temperature 1093 °C
2.43 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 160kg/m3; ASTM C201
 0.410 W/m-K
@Temperature 1093 °C
2.85 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 128kg/m3; ASTM C201
Maximum Service Temperature, Air 1343 °C2449 °FContinuous Use
 1427 °C2601 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 43 %43 %after firing
Cr2O3 3.0 %3.0 %after firing
SiO2 54 %54 %after firing
 
Descriptive Properties
Colorblue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool 80 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 3000 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Papers STD Paper Ceramic Fiber

CMORF70164 / 203462

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.