MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Borealis BorSafe™ HE3470-LS Black HDPE Compound for Pressure Pipes
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HE3470-LS is a black, high density polyethylene compound classified as an MRS 8.0 material (PE80) produced by the advanced Borstar technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system.

HE3470-LS is recommended for pressure piping system systems in the application field of drinking water, natural gas, pressure sewage, relining, sea outfall and industrial. The combination of high mechanical strength and excellent long term performance together with improved sagging performance makes it the ideal pressure pipe material.

Former trade name for this product was Borstar®.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.956 g/cc0.0345 lb/in³Compound; ISO 1183
Environmental Stress Crack Resistance >= 2000 hour
@Temperature 80.0 °C
>= 2000 hour
@Temperature 176 °F
At 8.0 bar; ISO 13479
Carbon Black Loading >= 2.0 %>= 2.0 %ASTM D1603
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psiAt 50 mm/min; ISO 527-2
Elongation at Break >= 600 %>= 600 %ISO 527-2
Tensile Modulus 1.00 GPa145 ksiAt 1 mm/min; ISO 527-2
 
Processing PropertiesMetricEnglishComments
Die Temperature 200 - 210 °C392 - 410 °F
Melt Temperature 200 - 220 °C392 - 428 °F
Head Temperature 200 - 210 °C392 - 410 °F
 
Descriptive Properties
Resistance to Rapid Crack Propagation, BAR8ISO 13477, Pc at 0°C, S4 / pipe size 250 mm SDR 11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Borealis Borstar® HE3474-LS Blue HDPE Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Drinking Water
Borealis Borstar® FB3450 HDPE for Film Extrusion
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications

PBOREA117 / 27424

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.