MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay SIPOMER® IBOMA-HP IsoBornyl Methacrylate
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: IsoBornyl Methacrylate

CAS: 7534-94-3

Available in: Asia Pacific, Europe, Latin America and North America.

Applications: SIPOMER IBOMA-HP is a High Tg, hydrophobic monomer improves toughness, water resistance and UV resistance

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity <= 20 cP#1 Spindle @ 60 rpm; RP-0596
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.15 %Karl fisher; RP-0327
 
Descriptive Properties
AppearanceClear, colorless liquidRP-0064
Assay>98.5%RP-0255
Color<30APHA, RP-0134
CompositionAcidity (as Methacrylic, 86)<0.1%, RP-0008
 MEHQ120-180 ppm, RP-1404
 PTZ<5.0 ppm, RP-1404

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay SIPOMER® WAM Allyl / Ureido Monomer
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate
Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate

WRHOD504 / 137735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.