MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Mindel® S-1000 Modified Polysulfone  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, Modified

Material Notes:

This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.

Key Words: PSU
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Water Absorption 0.20 %in 24 hours per ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 66.0 MPaASTM D638
Elongation at Break 100 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 2.41 GPaASTM D638
Flexural Yield Strength 97.0 MPaASTM D790
Flexural Modulus 2.63 GPaASTM D790
Izod Impact, Notched 0.900 J/cmASTM D256
Tensile Impact Strength 270 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 0.320 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 103 µm/m-°C
@Temperature 20.0 °C
ASTM E381
CTE, linear, Transverse to Flow 103 µm/m-°C
@Temperature 20.0 °C
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 149 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.30 mm
 V-0
@Thickness 3.30 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gharda Chemicals Gafone S 1500 Polysulfone (PS)
Avient Edgetek® PF-1000 Polysulfone
Westlake Plastics Thermalux® Polysulfone (PSU)
Syensqo (Solvay Specialty Polymers) Mindel® B-430 Polysulfone, Modified (PSU, Modified)
Syensqo (Solvay Specialty Polymers) Mindel® B-322 Polysulfone, Modified (PSU, Modified)

PSOLVT17 / 21313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.