MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Thermalux® Polysulfone (PSU)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: Thermalux® Polysulfone (PSU) is an amber colored, semi-transparent, heat-resistant, high performance engineering thermoplastic that offers higher heat resistance and better hydrolytic stability than polycarbonate (PC). It retains its good mechanical properties when exposed to steam and other sterilization techniques.

Industry: Chemical Process; Life Sciences; Semiconductor and ESD

Colors Available: Natural

Attributes: Dimensional Stability; Heat Resistant; Food Contact; Dielectric Properties; Transparent

Shapes: Extruded Slab; Compression Sheet; Extruded Rod; Extruded Sheet; Extruded Film

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Water Absorption 0.030 %
@Time 86400 sec
0.030 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 MPa10200 psiASTM D638
Elongation at Break 50 - 100 %50 - 100 %ASTM D638
Tensile Modulus 2.48 GPa360 ksiASTM D638
Flexural Strength 106 MPa
@Strain 5.0 %
15400 psi
@Strain 5.0 %
ASTM D790
Flexural Modulus 2.69 GPa390 ksiASTM D790
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.02e+6 ohm-cm1.02e+6 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FASTM D648
 
Descriptive Properties
ColorTransparent Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® PF-1000 Polysulfone
Gharda Chemicals Gafone S 1500 Polysulfone (PS)
Syensqo (Solvay Specialty Polymers) Mindel® S-1000 Modified Polysulfone
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade
Aclo Accutech Polypropylene Copolymer CP0437G40CL Glass Reinforced Coupled

PWEST121 / 72753

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.