MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Pressure Vessel Steel; Stainless Steel

Material Notes:

Applications:

  • Process equipment in chemical industry
  • Bleaching equipment in the pulp and paper industry
  • Flue-gas cleaning
  • Desalination
  • Seawater handling
  • Heat exchangers

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4547; UNS S31254
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell >= 210Hot rolled plate/Hot rolled strip/Cold rolled strip; EN 10003-1
Tensile Strength, Ultimate 680 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 510 MPa
@Temperature 400 °C
EN min.; EN 10002-5
 525 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 560 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 615 MPa
@Temperature 100 °C
EN min.; EN 10002-5
Tensile Strength, Yield 300 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 340 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 380 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 160 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 170 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 190 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 190 MPa
@Strain 1 %,
Temperature 400 °C
EN min.; EN 10002-5
 200 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 225 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 230 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 270 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 50 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Modulus of Elasticity 195 GPaRT
 166 GPa
@Temperature 400 °C
Poissons Ratio 0.30RT
Shear Modulus 75.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Hot rolled strip/Cold rolled strip; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000850 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 100 °C
 18.0 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 14.0 W/m-KRT
 18.0 W/m-K
@Temperature 400 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1120 - 1150 °C
@Thickness <=2.00 mm
Solution Annealing, cooling with air/water
 1150 - 1200 °C
@Thickness >=2.00 mm
Solution Annealing, quench with water
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.010 %
Chromium, Cr 20 %
Iron, Fe 55.69 %
Molybdenum, Mo 6.1 %
Nickel, Ni 18 %
Nitrogen, N 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 2205 Duplex Stainless Steel
Outokumpu 904L High Performance Austenitic Stainless Steel
Outokumpu 4565 High Performance Austenitic Stainless Steel
Type 254 SMO High-Nitrogen Austenitic Stainless Steel, Annealed Plate, Sheet, Strip, UNS S31254
Overview of materials for 2000 Series Aluminum Alloy

NOUTOK34 / 18749

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.