Finished product available as bar or wire. Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial. Information provided by Chicago Extruded Metals |
CDA 220, ASTM B36, ASTM B134, SAE J461, SAE J463 |