MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reade Advanced Materials Petalite Powder (Li2O·Al2O3·8SiO2)
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Description: Rare, light and fragile with tabular or columnar crystals. A monoclinic mineral with a framework silicate structure. Its color is creamy to white and sometimes to more rarely pinkish. It has a thermal expansion coefficient lower than almost any other inorganic or organic filler. An important ore of lithium. Used as a lithium addition glasses and porcelain enamels.
Forms Available: Sintered pieces, targets, and powder

Information provided by Reade Advanced Materials.

Key Words: Li2O·Al2O3·8SiO2, Lithium aluminum silicate, Aluminum lithium silicate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.350 - 2.470 g/cc0.08490 - 0.08924 lb/in³
pH 7.5 - 10.57.5 - 10.5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 6.0 - 6.56.0 - 6.520°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear -0.300 - 0.500 µm/m-°C
@Temperature 20.0 - 100 °C
-0.167 - 0.278 µin/in-°F
@Temperature 68.0 - 212 °F
Melting Point 1400 °C2550 °F
 
Descriptive Properties
Crystal Structuremonoclinic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Aperam N42 Cold Rolled Strip
3M Controltac™ 8620 ES Conformable Graphic Film
BNZ Materials Bazelite 2500 LI Insulating Castable
BYK Laponite® S485 Magnesium Aluminum Silicate

CREADE016 / 1950

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.