MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chesterton ARC 988 Composite
Categories: Other Engineering Material; Polymer

Material Notes: Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physical abuse. ARC 988 provides protection against chemical attack from highly aggressive substances including concentrated acids, alkalies and a wide variety of organic solvents. It is a trowelable overlayment which can be used at a thickness as low as 6 mm (1/4”). Its sag resistance makes it ideal for both vertical and horizontal applications. ARC 988 closes easily with a trowel, sealing the surface to prevent chemical attack on the substrate by permeation. The product produces a dense, fine textured surface. Non-shrinking 100% solids.

Benefits:

  • Protects concrete and provides chemical containment of concentrated acids such as sulfuric acid up to 98%
  • Fine textured sealed surface produces a tough, durable, chemical resistant, low maintenance overlayment
  • Compatible thermal coefficient of expansion provides long-term resistance to disbondment.
  • Moisture insensitive primer provides outstanding adhesion to damp concrete, a unique feature for concrete overlayments
  • User friendly consistency makes installation and finishing fast and easy
  • The reinforcement is engineered to minimize air entrapment and to improve mixing
  • ARC 988 is stronger than standard concrete, and its tough resin structure resists mechanical impact.

Applications: ARC 988 is generally used to repair and upgrade concrete surfaces or used as a replacement for acid resistant tiles , phenolics, furans, polyesters, sulfonated concretes and other overlayments. It is formulated to be thermally compatible with concrete. ARC 988 has the unusual ability to bond to damp concrete. ARC 988 is chosen over other ARC Composites for Concrete for its superior chemical resistance.

Suggested Uses:

  • Battery Rooms
  • Pickling & Plating Lines
  • Bleaching Areas
  • Sumps, Trenches & Pits
  • Chemical Containments
  • Pump & Equipment Bases
  • Concentrated Acid Areas
  • Waste Water Treatment

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.00 g/cc0.0723 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.7 MPa3000 psiASTM C370
Modulus of Elasticity 12.4 GPa1800 ksiASTM C580
Flexural Strength 37.9 MPa5500 psiASTM C580
Compressive Strength 97.9 MPa14200 psiASTM C579
Adhesive Bond Strength >= 2.76 MPa>= 400 psiExcellent - 100% Concrete
Abrasion <= 136<= 136[mg], Tabor, H-18/250gm wt/500 cycles
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM C531
Maximum Service Temperature, Air 66.0 °C151 °F(Water Immersion) Continuous
 93.0 °C199 °F(Water Immersion) Intermittent
 
Processing PropertiesMetricEnglishComments
Cure Time  90.0 min
@Temperature 32.0 °C
1.50 hour
@Temperature 89.6 °F
Foot Traffic
 120 min
@Temperature 25.0 °C
2.00 hour
@Temperature 77.0 °F
Foot Traffic
 180 min
@Temperature 32.0 °C
3.00 hour
@Temperature 89.6 °F
Light Load
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
Light Load
 300 min
@Temperature 16.0 °C
5.00 hour
@Temperature 60.8 °F
Foot Traffic
 480 min
@Temperature 16.0 °C
8.00 hour
@Temperature 60.8 °F
Light Load
 480 min
@Temperature 32.0 °C
8.00 hour
@Temperature 89.6 °F
Full Load
 780 min
@Temperature 25.0 °C
13.0 hour
@Temperature 77.0 °F
Full Load
 2040 min
@Temperature 16.0 °C
34.0 hour
@Temperature 60.8 °F
Full Load
 7200 min
@Temperature 32.0 °C
120 hour
@Temperature 89.6 °F
Full Chemical
 17300 min
@Temperature 25.0 °C
288 hour
@Temperature 77.0 °F
Full Chemical
 20200 min
@Temperature 16.0 °C
336 hour
@Temperature 60.8 °F
Full Chemical
 
Descriptive Properties
ColorGray
 Red
Thermal Compatibility to ConcretePassesASMT C884

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
Borosilicate Glass
Boron Nitride, Cubic BN, (Borazone)
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive

PPTCHS018 / 138130

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.