MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: Key Features:
  • Unfilled

Suitable processing methods:

  • Injection molding

Information provided by Bayer Polymers.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12.0 MPaStress at 50% Strain
Elongation at Break >= 50 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.30e+12 ohm-cm
Surface Resistance 3.00e+12 ohm
Dielectric Constant 4.5
@Frequency 1e+6 Hz
 5.5
@Frequency 100 Hz
Dielectric Strength 19.7 kV/mm
Dissipation Factor 0.027
@Frequency 100 Hz
 0.069
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 163 µm/m-°C
@Temperature 20.0 °C
Vicat Softening Point 145 °C50°C/h 50N
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 °CInjection Molding
Mold Temperature 30.0 °CInjection Molding
Injection Pressure 50.0 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Covestro Texin® 185 Urethane Thermoplastic Elastomer
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
Covestro Texin® 950 Urethane Thermoplastic Elastomer
Covestro Texin® 945U Urethane Thermoplastic Elastomer

PB10047 / 26085

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.