System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, 10% Glass Filled
Material Notes:
Polycarbonate with 10% glass fiber reinforcement
High stiffness, good impact resistance
Information provided by Cossa Polimeri S.r.l.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.26
g/cc
ASTM D 792
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
ASTM D 955
Melt Flow
8.0
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
60.0
MPa
ASTM D 638
Elongation at Break
4.0 %
ASTM D 638
Flexural Modulus
3600
MPa
ASTM D 790
Izod Impact, Notched
100
J/m
@Temperature 0.000 °C
ASTM D 638
120
J/m
@Temperature 23.0 °C
ASTM D 256
Thermal Properties
Original Value
Comments
Hot Ball Pressure Test
135
°C
I.E.C. 335-1
Vicat Softening Point
144
°C
@Load 5.00 kg
50°C/hr; ASTM D 1525
150
°C
@Load 0.999 kg
50°C/hr; ASTM D 1525
Flammability, UL94
V-2
@Thickness 1.60 mm
V-2
@Thickness 3.20 mm
Glow Wire Test
850
°C
@Thickness 2.00 mm
I.E.C. 695-2-1
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
RTP Company RTP 80309 Polycarbonate, Long Glass Fiber 50%
RTP Company RTP 303 FR Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release
PTS Tristar® PC-10GF-HC-V 10% Glass Fiber Polycarbonate
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release
PCOSSA849 / 156439
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.