Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistance to chemicals. Applications: Engineering and insulation material in large rotating electrical machines and insulation cylinders in dry transformers. Information provided by Elektro-Isola |
IEC/EN 61212-3-1 EP GC 22, DIN 7735 Hgw 2375.4, NEMA LI G-11 |