MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BS 970 080M40 Carbon Steel
Categories: Metal; Ferrous Metal; British Designations; Carbon Steel; Medium Carbon Steel

Material Notes: This British mild steel is very similar to the American AISI 1040 mild steel. Refer to AISI 1040 for additional properties.

Key Words: EN8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccTypical Carbon Steel
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 146 - 197
@Diameter 150 - 250 mm
normalized bright bar
Tensile Strength, Ultimate 660 MPa6-13mm, hot rolled, cold drawn bright bar
 510 MPa
@Diameter 150 - 250 mm
normalized bright bar
Tensile Strength, Yield 530 MPa6-13mm, hot rolled, cold drawn bright bar
 245 MPa
@Diameter 150 - 250 mm
normalized bright bar
Elongation at Break 7.0 %6-13mm, hot rolled, cold drawn bright bar
 17 %
@Diameter 150 - 250 mm
normalized bright bar
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.36 - 0.44 %
Iron, Fe >= 97.91 %
Manganese, Mn 0.60 - 1.0 %
Molybdenum, Mo <= 0.15 %
Phosphorus, P <= 0.050 %
Silicon, Si 0.10 - 0.40 %
Sulfur, S <= 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1018 Steel, cold drawn
AISI 1040 Steel, as rolled
AISI 1016 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
Goodfellow Carbon/Epoxy Composite Sheet
Iron, Fe

MBS080M40A / 10335

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.