Availability: Europe; Asia Pacific; North America Additive: Heat Stabilizer; Lubricant Features: General Purpose; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Uses: Appliances; Automotive Applications; Electrical/Electronic Applications Agency Ratings: UL 94 Automotive Specifications: CHRYSLER MS-DB-41 CPN1899 Color: BK001 Black; FORD ESF-M4D82-A Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |