MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Chemlon® 100 H Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Availability: Europe; Asia Pacific; North America

Additive: Heat Stabilizer; Lubricant

Features: General Purpose; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated

Uses: Appliances; Automotive Applications; Electrical/Electronic Applications

Agency Ratings: UL 94

Automotive Specifications: CHRYSLER MS-DB-41 CPN1899 Color: BK001 Black; FORD ESF-M4D82-A

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.015 - 0.022 cm/cm0.015 - 0.022 in/inASTM D955
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 275 °C
10 g/10 min
@Load 0.716 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 50 %50 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 0.862 GPa125 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.86 GPa415 ksiASTM D790
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 18.1 kV/mm
@Thickness 3.00 mm
460 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 600 V600 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.2 µm/m-°C39.0 µin/in-°FASTM D969
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FUnannealed; ASTM D648
UL RTI, Electrical  95.0 °C
@Thickness 0.762 mm
203 °F
@Thickness 0.0300 in
UL 746
 105 °C
@Thickness 1.52 mm
221 °F
@Thickness 0.0600 in
UL 746
 110 °C
@Thickness 3.05 mm
230 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical with Impact  95.0 °C
@Thickness 0.762 mm
203 °F
@Thickness 0.0300 in
UL 746
 105 °C
@Thickness 1.52 mm
221 °F
@Thickness 0.0600 in
UL 746
 110 °C
@Thickness 3.05 mm
230 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical without Impact  110 °C
@Thickness 0.762 mm
230 °F
@Thickness 0.0300 in
UL 746
 110 °C
@Thickness 1.52 mm
230 °F
@Thickness 0.0600 in
UL 746
 110 °C
@Thickness 3.05 mm
230 °F
@Thickness 0.120 in
UL 746
Flammability, UL94 V-2
@Thickness 0.762 mm
V-2
@Thickness 0.0300 in
Oxygen Index 27 %27 %ASTM 2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 241 - 254 °C465 - 490 °F
Middle Barrel Temperature 257 - 271 °C495 - 520 °F
Front Barrel Temperature 263 - 282 °C505 - 540 °F
Nozzle Temperature 263 - 279 °C505 - 535 °F
Melt Temperature 257 °C495 °F
 263 - 279 °C505 - 535 °F
Mold Temperature 21.1 - 93.3 °C70.0 - 200 °F
Drying Temperature 79.4 °C175 °F
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0423 / 236914

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.