MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EN S355J0 High Manganese, Structural, Hot Rolled, Quality Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Key Words: EN 10025(90)A1(93) S355J0. Similar to ASTM A678(C), UNS K02204
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/ccEstimated by MatWeb from similar grade
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 450 - 630 MPa
@Thickness 200 - 250 mm
 490 - 630 MPa
@Thickness 3.00 - 16.0 mm
 490 - 630 MPa
@Thickness 63.0 - 80.0 mm
 510 - 680 MPa
@Thickness <=1.00 mm
Tensile Strength, Yield 285 MPa
@Thickness 200 - 250 mm
 335 MPa
@Thickness 63.0 - 80.0 mm
 355 MPa
@Thickness 3.00 - 16.0 mm
 355 MPa
@Thickness <=1.00 mm
Elongation at Break 12 %
@Thickness <=1.00 mm
Transverse
 14 %
@Thickness <=1.00 mm
Longitudinal
 17 %
@Thickness 200 - 250 mm
Longitudinal
 17 %
@Thickness 200 - 250 mm
Transverse
 18 %
@Thickness 63.0 - 80.0 mm
Transverse
 20 %
@Thickness 63.0 - 80.0 mm
Longitudinal
 20 %
@Thickness 3.00 - 16.0 mm
Transverse
 22 %
@Thickness 3.00 - 16.0 mm
Longitudinal
Modulus of Elasticity 200 GPaEstimated by MatWeb from similar grade
Poissons Ratio 0.29Estimated by MatWeb from similar grade
Shear Modulus 80.0 GPaEstimated by MatWeb from similar grade
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000170 ohm-cmEstimated by MatWeb from similar grade
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°CEstimated by MatWeb from similar grade
Specific Heat Capacity 0.470 J/g-°CEstimated by MatWeb from similar grade
Thermal Conductivity 52.0 W/m-KEstimated by MatWeb from similar grade
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.20 %
@Thickness <=16.0 mm
CEV may be required.
 <= 0.22 %
@Thickness >=63.0 mm
CEV may be required.
Iron, Fe >= 97.5 %
Manganese, Mn <= 1.6 %
Nitrogen, N <= 0.0090 %N max n/a if Al >= 0.020
Phosphorus, P <= 0.040 %
Silicon, Si <= 0.55 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4130 Steel, normalized at 870°C (1600°F)
3M PS470 White Yupo™ EDP Label Product
ASTM A678 Steel, grade C
EN S275J0 High Manganese, Structural, Hot Rolled, Quality Steel, t>200 mm
EN S355J2G3C High Manganese, Structural, Hot Rolled, Quality Steel

M9ZES355J0 / 233233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.