MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection Molding

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
Tensile Strength at Break 29.42 MPa
Elongation at Break 900 %
100% Modulus 0.00440 GPa
@Strain 100 %
300% Modulus 0.00590 GPa
@Strain 300 %
Resilience 50%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 25
 
Processing PropertiesOriginal ValueComments
Feed Temperature 165 °C
Middle Barrel Temperature 170 °CCompress zone
Front Barrel Temperature 175 °CMetering zone
Adapter Temperature 180 °C
Die Temperature 356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade
Wanhua Chemical Wanthane® WHT-8280H Super Hard Polyether-Based TPU
Covestro Texin® 288 Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 9885DU TPU

PTPU36 / 70892

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.