MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: High Hydrolysis resistance and good crystallinity. Suggested for extrusion.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D995
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Hardness, Shore D 3535ASTM D2240
Tensile Strength at Break 40.0 MPa5800 psiDIN 53504
Elongation at Break 800 %800 %ASTM D412
100% Modulus 5.50 MPa
@Strain 100 %
798 psi
@Strain 100 %
DIN 53504
300% Modulus 12.6 MPa
@Strain 300 %
1830 psi
@Strain 300 %
DIN 53504
Rebound 36 %36 %Bayshore; ASTM D2632
Tear Strength 105 kN/m600 pliASTM D624
Abrasion 3030[mm3]; ISO 4649
Compression Set  19 %
@Temperature 23.0 °C,
Time 252000 sec
19 %
@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
 36 %
@Temperature 70.0 °C,
Time 86400 sec
36 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 5.00e+8 ohm5.00e+8 ohmantistat
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 - 175 °C329 - 347 °FHuntsman/TMA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 288 Thermoplastic Polyurethanes (TPU)
Covestro Desmopan® 9885DU TPU
Taiwan PU Corporation TPUI-L70 Low Temperature Resistance, Injection Molding Polyester Base TPU
Wanhua Chemical Wanthane® WHT-8280H Super Hard Polyether-Based TPU
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer

PHU9915 / 150375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.