MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Heat Resistant

Material Notes: Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion Grade

Features: • Bromine Free • Chlorine Free
Process: Extrusion
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219; Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 4.0 - 8.0 g/10 min
@Load 11.6 kg,
Temperature 250 °C
4.0 - 8.0 g/10 min
@Load 25.6 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 119119ASTM D785
Tensile Strength at Break 62.1 MPa9000 psiASTM D638
Tensile Strength, Yield 64.1 MPa9300 psiASTM D638
Flexural Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 2.41 GPa350 ksiASTM D790
Izod Impact, Notched  1.33 J/cm
@Temperature -40.0 °C
2.50 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 2.14 J/cm
@Temperature 22.8 °C
4.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 16.9 J12.5 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Dielectric Strength 24.0 kV/mm
@Thickness 3.00 mm
610 kV/in
@Thickness 0.118 in
ASTM D149
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746
Hot Wire Ignition, HWI  >= 120 sec
@Thickness 1.50 mm
>= 120 sec
@Thickness 0.0591 in
UL 746
 >= 120 sec
@Thickness 1.70 mm
>= 120 sec
@Thickness 0.0669 in
UL 746
 >= 120 sec
@Thickness 3.00 mm
>= 120 sec
@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
UL 746
 60 - 120 arcs
@Thickness 1.70 mm
60 - 120 arcs
@Thickness 0.0669 in
UL 746
 60 - 120 arcs
@Thickness 3.00 mm
60 - 120 arcs
@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C265 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
UL RTI, Electrical  65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 1.70 mm
230 °F
@Thickness 0.0669 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 110 °C
@Thickness 1.70 mm
230 °F
@Thickness 0.0669 in
UL 746
 110 °C
@Thickness 3.00 mm
230 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.749 mm
149 °F
@Thickness 0.0295 in
UL 746
 105 °C
@Thickness 1.50 mm
221 °F
@Thickness 0.0591 in
UL 746
 105 °C
@Thickness 1.70 mm
221 °F
@Thickness 0.0669 in
UL 746
 105 °C
@Thickness 3.00 mm
221 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-1
@Thickness 1.50 mm
V-1
@Thickness 0.0591 in
 V-1
@Thickness 3.00 mm
V-1
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature >= 204 °C>= 400 °F
Middle Barrel Temperature >= 227 °C>= 440 °F
Front Barrel Temperature >= 227 °C>= 440 °F
Melt Temperature 227 - 254 °C440 - 490 °F
Drying Temperature 104 - 110 °C220 - 230 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.00254 cm0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Iupital® A10-03 Copolymer Acetal
Ineos N01N-00 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer
Ineos N00N-00 Polypropylene Impact Copolymer
Ineos N00M-00 Polypropylene Impact Copolymer

PPOLYQ206 / 160727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.