MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Xantar® C MC 3700 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: XANTAR® C properties are: Highest flow in combination with excellent toughness. High level of purity. High stability. Bright natural color. The benefits are: easier filling of complex parts, lower mould deposit during injection molding, low volatiles level and reduced fogging tendency, better long-term property retention and improved color consistency and appearance.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/cc
Melt Density 1.03 g/cc
@Temperature 280 °C
Water Absorption 0.50 %
Moisture Absorption 0.200 %
Linear Mold Shrinkage, Flow 0.0060 cm/cm
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min Volumetric Rate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPa
Elongation at Break >= 50 %
Elongation at Yield 5.0 %
Tensile Modulus 2300 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Constant 2.9
@Frequency 1e+6 Hz
Dielectric Strength 35.0 kV/mm
Comparative Tracking Index 275 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
CTE, linear, Transverse to Flow 70.0 µm/m-°C
Specific Heat Capacity 2.28 J/g-°Cmelt
Thermal Conductivity 0.230 W/m-Kmelt
Hot Ball Pressure Test 125 °C
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
Vicat Softening Point 130 °C
@Load 5.10 kg
rate 50°C/h
Glow Wire Ignition Temperature 725 °C
@Thickness 3.00 mm
 775 °C
@Thickness 1.50 mm
Glow Wire Flammability Index 700 °C
@Thickness 3.00 mm
 750 °C
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CAs Tested; Injection
Mold Temperature 80.0 °CAs Tested; Injection
Ejection Temperature 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Xantar® C MC 3650 Polycarbonate
Mitsubishi Xantar® C MC 3440 Polycarbonate
Mitsubishi Xantar® C MC 3433 Polycarbonate
Mitsubishi Xantar® C MC 3652 Polycarbonate
Toho Tenax Besfight® MC Type I (12,000 Filament) Nickel Coated Carbon Fiber

PMITSU9327 / 192001

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.